Fin density is optimally designed to accommodate high air pressure. The cooling performance improves significantly with increased fan speed, offering exceptional cooling performance during operation. FPI (fin per inch): 14.
German-Made Anti-Corrosion Materials
Without compromise, the Pacific RL Radiator Series is designed with high-quality German aerospace-grade materials and constructed with zinc, the most common anti-corrosion agent. Although this protection will gradually degrade as the zinc corrodes away over time, it provides the best means to reduce electronic conductivity and can withstand scratches to the zinc layer. Corrosion potentials of aluminum alloy with zinc can be reduced by 55.6% after brazing.
High-Quality Manufacturing Process: Brazing
An exceptional manufacturing process using high temperature brazing at 1022/550 sets Pacific RL Radiators in a class of their own. This technique allows for impurities to be kept out of the brazing process, ensuring that full strength on all the connected areas is achieved.
The radiators are baked through a controlled atmosphere brazing line. The materials melt into each other to accomplish optimal thermal transfer from the tubes to the actual fins in order to attain better heat evacuation.
Specifications
P/N |
CL-W014-AL00BL-A |
Dimension |
522.5 (L) x129 (W) x 64 (H) |
Weight |
1242g |
Material |
Anti-Corrosion Aluminum Alloy
|
FPI (Fin per inch) |
14
|
Flat Tube |
13 set
|
Screw Thread |
G 1/4 * 5
|
Parts |
Stopper *3 (G 1/4 ) |